Hi:
I want to make a hollow tube for an aerobar shaped lik " _/ "
I was thinking on making it with an inflatable blader and a epoxy mould sliced in 2.
What do you recomend?
By ArturK
-
5/25/2018 8:09:37 AM
Find at google "Piercan" company from France , we met them at JEC.
They are making bladders for the carbon fiber compistes.