v4chris
v4chris
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 8
Does easy lease have a shelf life?
I am having all sorts of problems getting your infusion resin to release from your uni-mould product.
I have lost several moulds and plugs now, and can only put it down to the release agent.
I bought the current batch of easy lease from you over a year ago now, does it lose its effectiveness?
Reply
Like
5
Reply
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Pretty sure Easy- Lease is Hygroscopic so it will absorb moisture from the surrounding area (once open to the atmosphere) I would think any moisture absorbed will have an adverse effect on the Easy-Lease. I always put the cap on between applications and then put the tin in the re-sealable bag that it came in from EC at the end of the day.
I am sure someone from EC will give a much better answer shortly.
Warren
Carbon
Copies Ltd
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Easy lease shelf life
v4chris
-
13 Years Ago
Pretty sure Easy- Lease is Hygroscopic so it will absorb moisture from the surrounding area (once...
wozza
-
13 Years Ago
Warren is right. The recommended shelf life is 1 year in a sealed container. If you havent used the...
Warren (Staff)
-
13 Years Ago
Just ordered some replacement easy lease and it works perfectly. Has been expensive though for me...
v4chris
-
13 Years Ago
That might be my problem also, damn shame on this lost mold :angry:
prsw
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search