Does easy lease have a shelf life?

I am having all sorts of problems getting your infusion resin to release from your uni-mould product.

I have lost several moulds and plugs now, and can only put it down to the release agent.
I bought the current batch of easy lease from you over a year ago now, does it lose its effectiveness?