wochi
wochi
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 31,
Visits: 188
Hi all!
I´m doing my first jobs in carbon and i´m having some problems.
When applying the first coat of resin to the mold, it won´t stick and i can´t make an even coat. When curing it starts to make voids in the middle of the mould. Probably because of the release agent. How can i fix this? I tried to make the part anyway and a got tons of holes in the surface like you can see in the photo.
Any help would be appreciated.
Thank you!
Reply
Like
2
Reply
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
everything is simple i have same nonsence!
you need to change first piece of cloth that you clean surface as it has wax inside until i not changed everytime was same like on your photo.
or also nefrase that you cleaning surface after brushing as some bad things from cleaning cloth can be into that. BUT I KNOW THAT GOONA BE CLEANING BAD CLOTH! CHANGE AND YOU BE GOOD.
or if piece you lay resin from mold or infusion then that mean surface has wax so resin not stick and act like this!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
First try, first problems
wochi
-
12 Years Ago
Hello The chemical release agents are very slick so its impossible to brush a layer down and have it...
fgayford
-
12 Years Ago
Thanks for your answer. I followed the steps in the laminatating video from carbonmods. So what i...
wochi
-
12 Years Ago
i tried to apply a coat on top of the part just to see the result and the same thing is happening....
wochi
-
12 Years Ago
everything is simple i have same nonsence! you need to change first piece of cloth that you clean...
TomDesign
-
12 Years Ago
It´s a possibility in this last photo as i wasn´t to cautious with the cleaning. was just a test....
wochi
-
12 Years Ago
Hi looking at the second picture this looks like what you call fish eyes, there is maybe silicone or...
Paulh37
-
12 Years Ago
What I think your problem is on the second picture is that you did not clean the part so there was...
matthieutje65
-
12 Years Ago
From my experience wet lay up will never yield perfect cosmetic parts alway hit and miss,infusion is...
Shaneer22
-
12 Years Ago
I do a fair bit of wetlay / vacbag stuff. I have also encountered this problem. Firstly the layer of...
FLD
-
12 Years Ago
thanks for all your help. I did what FLD suggested in this last post with the pinholes. Just flood...
wochi
-
12 Years Ago
I had similar problems. I got my best results by changing into vinilester clear gelcoat. It´s...
Zorongo
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search