Thickness- number of CF layers for motorbike fairing ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
thanxx Warren, I'll try again, with less pressure on the gun
Reply
Like
3
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Jess8bit (25/07/2013)
yeah, I totally agree, and I do the same.
I was nearly sure about you using sprayed GC on this one, because I recognize slight prints through it, marking the cloth, don't know if you see what i mean. The cloth is not completely flat, due to slight spots left by the spray gun.
This is a concern to me, as I'd like a perfect cosmetic part, and I'm looking for a solution to get rid of that.
A solution would be to slightly sand the GC once cured, to flatten it.
Sounds like you are either laying down the GC50 too thick or with too much air pressure. If applied correctly you should not need to sand it before lay-up, sort of defeats the object of using it in the first place.
Carbon
Copies Ltd
Edited
13 Years Ago by
wozza
Reply
Like
2
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
Bartonphoenix750 (25/07/2013)
Hi
it may be an issue with the image but the part came out quite well and the finish of the g50 was relatively flat prior to laying up the
carbon.
ok
Reply
Like
3
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
I use 2 layers of 245gr all over and a third on the perimeter. I will add another 3 or 4 layers where items fasten or strips where I need to reduce flex from wind ect....
The total weight is sub 1Kg...
The second photo shows some heavier carbon which was 400gr but I stopped using it as I ran out of the 400gr pre-preg and didnt want to buy 25sq m just for reinforcements..
Edited
13 Years Ago by
morepower
Reply
Like
3
carbonfibreworks
carbonfibreworks
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi
it may be an issue with the image but the part came out quite well and the finish of the g50 was relatively flat prior to laying up the
carbon.
Reply
Like
3
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
yeah, I totally agree, and I do the same.
I was nearly sure about you using sprayed GC on this one, because I recognize slight prints through it, marking the cloth, don't know if you see what i mean. The cloth is not completely flat, due to slight spots left by the spray gun.
This is a concern to me, as I'd like a perfect cosmetic part, and I'm looking for a solution to get rid of that.
A solution would be to slightly sand the GC once cured, to flatten it.
Reply
Like
2
carbonfibreworks
carbonfibreworks
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi
I used G50 and the EC spray gun, for me the finish of the mould is critical for producing a good part and reducing the time needed to polish the part etc.
Regards Chris
www.carbonfibreworks.co.uk
Reply
Like
2
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
Nice Barton !
Could you tell me if you used gel coat and how you have applied it ? (I would bet yes).
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Looks good!!
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
carbonfibreworks
carbonfibreworks
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Here is a front mudguard I made earlier, it has had the excess carbon removed and has yet to be polished. I used infusion and three layers of 200g carbon and a strip of core material to reduce torsional flex.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
1
2
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search