Hello guys

i made hoods with wrap of carbon with vaccuming and bag but like you can see from bag surface from resin become like this and i can not brush it till it dissapearment and if i lay epoxy on top it seems like carbon was cutted like with knife. any help that i can fix that ?http://www.talkcomposites.com/Uploads/Images/c31c612e-0ca8-4f9e-97c4-6592.jpghttp://www.talkcomposites.com/Uploads/Images/589677fe-0052-44fa-8c27-737c.jpg
Reply
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K






This is after i fixed damaged and need rewrap see bad side around its crazy to do by hands and i done lots of stuff only hands but that is to big for me that is why used vacuuming
Edited 12 Years Ago by TomDesign