Hello guys

i made hoods with wrap of carbon with vaccuming and bag but like you can see from bag surface from resin become like this and i can not brush it till it dissapearment and if i lay epoxy on top it seems like carbon was cutted like with knife. any help that i can fix that ?http://www.talkcomposites.com/Uploads/Images/c31c612e-0ca8-4f9e-97c4-6592.jpghttp://www.talkcomposites.com/Uploads/Images/589677fe-0052-44fa-8c27-737c.jpg
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Why are you using a vacuum bag? I think you would be OK doing it the normal way with a resin down then laying the carbon over the top. Then adding carbon and building up layers of resin to build your clear coat or use a clear gel coat over the carbon until you get the correct thickness and then polish up the surface.

http://youtu.be/6rTWaV1imzs
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
everything simple i have to wrap 2 hoods from both sides in carbon that way one side not a problem by hands other side 1 piece around unreal to do with hands. 

so how i can correct these things after you see i removed vacuming bag and surface like this i brushed dry paper 120 but it can not brush all lines and if im laying new resin on top i see on those places like cutted material lines.



can anyone help to save my work and materials with any advise? more then beer is reward!!
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K






This is after i fixed damaged and need rewrap see bad side around its crazy to do by hands and i done lots of stuff only hands but that is to big for me that is why used vacuuming
Edited 12 Years Ago by TomDesign
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search