Problem need help with carbon wrap
Problem need help with carbon wrap
Post Reply
Like
2
Problem need help with carbon wrap
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Hello guys
i made hoods with wrap of carbon with vaccuming and bag but like you can see from bag surface from resin become like this and i can not brush it till it dissapearment and if i lay epoxy on top it seems like carbon was cutted like with knife. any help that i can fix that ?
Reply
Like
2
Reply
morepower
morepower
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
Why are you using a vacuum bag? I think you would be OK doing it the normal way with a resin down then laying the carbon over the top. Then adding carbon and building up layers of resin to build your clear coat or use a clear gel coat over the carbon until you get the correct thickness and then polish up the surface.
http://youtu.be/6rTWaV1imzs
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Problem need help with carbon wrap
TomDesign
-
12 Years Ago
Why are you using a vacuum bag? I think you would be OK doing it the normal way with a resin down...
morepower
-
12 Years Ago
everything simple i have to wrap 2 hoods from both sides in carbon that way one side not a problem...
TomDesign
-
12 Years Ago
...
TomDesign
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search