Sorry to hear of this one,
I think we have all been there at some point, being impatient and trying to release a component too soon is easily done, it's worth noting that our fast and slow hardeners are compatible with eachother so you can mix them together at any ration to get different speeds.
Paul Statham Easy Composites / Carbon Mods - Technical
|