after returning from work i found my part had still not cured properly. i done it at 10 pm last night. i decided to remove it as i assume something wasnt right. its also stuck to the mould slightly as it hadnt cured properly and theres some epoxy still stuck to the mould.
did i mix the epoxy wrong? i only needed a small amount so i decided to mix 12.5 grams so 9.5 grams epoxy and 3 grams hardner. is this correct?
checked the site and according to the specs of this slow resin i should have left it 24hrs

my bad
think ill purchase fast hardner as i need it to cure faster lol.