after returning from work i found my part had still not cured properly. i done it at 10 pm last night. i decided to remove it as i assume something wasnt right. its also stuck to the mould slightly as it hadnt cured properly and theres some epoxy still stuck to the mould.

did i mix the epoxy wrong? i only needed a small amount so i decided to mix 12.5 grams so 9.5 grams epoxy and 3 grams hardner. is this correct?

checked the site and according to the specs of this slow resin i should have left it 24hrs Sad my bad

think ill purchase fast hardner as i need it to cure faster lol.


Edited 13 Years Ago by japcarmaniac
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search