carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
yes
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
dam so cactus why others waiste time and work and sand parts if result be the same.??
Reply
Like
5
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
You have to sand to get rid of any high spots.
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
do not understand. i can lay polyster on part then brush till 3000 paper and simply polish correct? no need laquer as you told uv protected?
Also please link for polyster resin you told as i called our guys not have that resin!
Reply
Like
5
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
Are you in the UK or Poland? I know several suppliers in both countries
Edited
13 Years Ago by
carboncactus
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
in lithuania
Reply
Like
5
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
You just need to ask for a polyester gel coat and get a good quality one...
http://www.ecfibreglasssupplies.co.uk/p-1483-clear-polyester-gel-coat-inclusive-of-catalyst.aspx
This is a crystic 65PA gel coat... So if you have a Scott Bader supplier they will have it..
Reply
Like
5
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
im sorry you told polyster resin to lay on part and polish not to lay polyster-gelcoat! so i not understand you.
Reply
Like
5
Greg
Greg
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 353
All polyesters resistant for UV?
I don't think so, When I start work at composites I made some parts from polyester, all stayed matt look much faster than epoxy resins, but It was the cheapest polyester resin on the market about 1,25€ per kg.
Polyesters have one advantge than epoxy it can be polished many times and will be look like new.
Reply
Like
5
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
TomDesign (25/06/2013)
im sorry you told polyster resin to lay on part and polish not to lay polyster-gelcoat! so i not understand you.
Here is the resin too...
http://www.ecfibreglasssupplies.co.uk/p-1531-lloyds-approved-polyester-resin-including-catalyst.aspx
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Prev
1
4
5
6
7
8
9
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search