Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Other
»
Carbon Fibre Tea Tray
Carbon Fibre Tea Tray
Post Reply
Like
6
Prev
1
3
4
5
6
7
9
Next
Jump To Page
Carbon Fibre Tea Tray
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
please numbers of resin that way i know which is bad and which is uv protected like you say?
Reply
Like
4
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
carboncactus (25/06/2013)
morepower (25/06/2013)
PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....
Which resin system and Diolen weight would it be? I quoted for 25m of 265g on RF464 (low temp)
That is fine.. It is the stuff I used last time with the VTF suface and the SHD backing material and it was compatible with both..
Reply
Like
4
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
TomDesign (25/06/2013)
PLEASE NUMBER OF RESIN OR SMTH AS MARINE RESIN NO ONE SELL HERE
Any Lloyds approved resin is fine and almost all polyester resin is UV stable. I use lloyds approved from a number of suppliers like Eastcoast Fibreglass or MBFG.
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
PLEASE NUMBER OF RESIN OR SMTH AS MARINE RESIN NO ONE SELL HERE
Reply
Like
3
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
WARREN I NEED MANUFACTURER OR NUMBER OF RESIN SO I ASK PEOPLE HERE AS NO ONE SELL MARINE RESIN!
Reply
Like
4
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
morepower (25/06/2013)
PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....
Which resin system and Diolen weight would it be? I quoted for 25m of 265g on RF464 (low temp)
Edited
13 Years Ago by
carboncactus
Reply
Like
3
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Any Marine grade Polyester will give good U.V protection.
Carbon
Copies Ltd
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
STILL NO REPLY PLEASE LET ME KNOW WHICH POLYSTER RESIN YOU USE OR ANY LINK THAT NOT NEED CLEAR COAT ONLY POLISHING??
Reply
Like
4
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
carboncactus (24/06/2013)
morepower (24/06/2013)
I use pre-preg Diolen ...
I need some prepreg Diolen sharpish. Just emailed PRF for a quote on a 25m roll, but only need about 5 metres. Let me know if you wanna do a group buy. I'm gonna have to get a roll of VTF as well soon....
How are you doing for VTF?
Bear with me...lol... I have a little issue with a customer of our mutual friend.... he paid for a kit direct to ****s and then didnt want to pay more... Now he does.. so it is an on/off/on sale so as he didnt want the kit I sold it as it was taking up space... So it looks like I will need some more...Of both..... PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....
Reply
Like
4
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
morepower (24/06/2013)
I use pre-preg Diolen ...
I need some prepreg Diolen sharpish. Just emailed PRF for a quote on a 25m roll, but only need about 5 metres. Let me know if you wanna do a group buy. I'm gonna have to get a roll of VTF as well soon....
How are you doing for VTF?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Prev
1
3
4
5
6
7
9
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search