TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
STILL NO REPLY PLEASE LET ME KNOW WHICH POLYSTER RESIN YOU USE OR ANY LINK THAT NOT NEED CLEAR COAT ONLY POLISHING??
Reply
Like
6
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Any Marine grade Polyester will give good U.V protection.
Carbon
Copies Ltd
Reply
Like
5
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
morepower (25/06/2013)
PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....
Which resin system and Diolen weight would it be? I quoted for 25m of 265g on RF464 (low temp)
Edited
13 Years Ago by
carboncactus
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
WARREN I NEED MANUFACTURER OR NUMBER OF RESIN SO I ASK PEOPLE HERE AS NO ONE SELL MARINE RESIN!
Reply
Like
5
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
PLEASE NUMBER OF RESIN OR SMTH AS MARINE RESIN NO ONE SELL HERE
Reply
Like
5
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
TomDesign (25/06/2013)
PLEASE NUMBER OF RESIN OR SMTH AS MARINE RESIN NO ONE SELL HERE
Any Lloyds approved resin is fine and almost all polyester resin is UV stable. I use lloyds approved from a number of suppliers like Eastcoast Fibreglass or MBFG.
Reply
Like
6
morepower
morepower
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
carboncactus (25/06/2013)
morepower (25/06/2013)
PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....
Which resin system and Diolen weight would it be? I quoted for 25m of 265g on RF464 (low temp)
That is fine.. It is the stuff I used last time with the VTF suface and the SHD backing material and it was compatible with both..
Reply
Like
5
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
please numbers of resin that way i know which is bad and which is uv protected like you say?
Reply
Like
6
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
Any polyester will protect against UV. When cured, the ester groups create benzene rings which absorb UV light.
Reply
Like
4
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
so cactus you say i wrap part i lay polyster clear and polish and perfect hard finish and uv protected and not appear any white spots from sun and etc?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Prev
1
3
4
5
6
7
9
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search