Let's say you have a bonnet you want to skin with carbon. How to prepare the surface (which is obviously made of paint and clear coat) ?

Do you proceed the exact same way as for a plastic part (as shown in the Carbon Mods tutorial video) where you start with sand the part ?

Is making such a big surface not too risky ??

thank you Smile

Jess
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You still need to rough the surface to ensure good adhesion between the base coat and the bonnet.

People have successfully skinned bonnets and other large panels before, although I recommend a small piece to start with or work on a spare panel from the scrap yard in case it goes wrong.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Warren (Staff) (14/06/2013)
You still need to rough the surface to ensure good adhesion between the base coat and the bonnet.

People have successfully skinned bonnets and other large panels before, although I recommend a small piece to start with or work on a spare panel from the scrap yard in case it goes wrong.
Ok Warren,

Which grit would use ? 120 ? 240 ?
...and, which depth should I sand down to ? (do I aim at sanding clear coat only ? or till paint ? metal ?)

Also, would you be so kind as to point me towards the material list I woud need to order from the EC store ? (I mean the different resins required to do skinning) for about the size of a complete car BigGrin Blush