Issue applying PVA over release wax on mould


Author
Message
Trevor Harris
Trevor Harris
Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)
Group: Forum Members
Posts: 22, Visits: 116
Hi,

    Have made first mould with high surface finish and applied 5 coats of release wax. Applied PVA with sponge to get an even coat. OK for a few moments then it forms into droplets, which is what you would expect when applying a liquid over a waxed surface but surely this will impact on surface finish of gel coat ? I tried again with a brush and the same effects. Any advice gratefully received.

Trevor
Replies
Shaneer22
Shaneer22
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Don't waist your time use semipermanent release agent.  The only time I use wax is on plugs. 
Trevor Harris
Trevor Harris
Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)
Group: Forum Members
Posts: 22, Visits: 116
Hi Shaneer22,

                       What I am calling a mould is what I think you would call a plug. A spray painted MDF male mould to make a female  master from epoxy mould making putty and tooling gel coat.

Trevor