By Trevor Harris - 5/28/2013 10:59:39 AM
Hi,
Have made first mould with high surface finish and applied 5 coats of release wax. Applied PVA with sponge to get an even coat. OK for a few moments then it forms into droplets, which is what you would expect when applying a liquid over a waxed surface but surely this will impact on surface finish of gel coat ? I tried again with a brush and the same effects. Any advice gratefully received.
Trevor
|
By Trevor Harris - 5/29/2013 9:33:58 AM
Hi Fred, Carbon Cactus and Shaneer,
Thanks for the advice. It is helpful to get several perspectives on a problem
Trevor
|
|