How many parts should I expect to be able to pull from a Uni Mould? What's the limiting factor?

Thanks,
James
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8K
plus remember you can easily polish back up the surface finish if that dulls.

We have Uni-mould tools that have had hundreds of pulls from.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search