By jamesw - 5/17/2013 7:32:10 PM
How many parts should I expect to be able to pull from a Uni Mould? What's the limiting factor?
Thanks, James
|
By Warren (Staff) - 5/20/2013 9:43:44 AM
plus remember you can easily polish back up the surface finish if that dulls.
We have Uni-mould tools that have had hundreds of pulls from.
|
|