Gel coat before Infusion


Author
Message
Nick Igoe
Nick Igoe
Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)
Group: Forum Members
Posts: 12, Visits: 118
You can do this if you are confident that the gel coat is not going to pool in any crevasses as this will make the part look resin rich in those areas assuming you are using a clear gel coat.

Far UK
huug
huug
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 1, Visits: 2
Hello, 

Do you think it's a good idea to first add a layer of clear gel coat to mould before infusion.
The idea is to better protect against UV and prevent fibers getting to the surface.

Yours, 

Huug
Tags
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search