Hi,
I'm planning on building a 3D rock background out of polystyrene to place inside my aquarium.  The plan is to sculpt and shape the polystyrene 'rocks', stick them individually onto a thin flat polystyrene backing sheet and then brush it with several epoxy resin coats (with suitable dyes if needed) to achieve the right colours and a bit of strength (the polystyrene itself is inert and does not need to be sealed off completely from the aquarium water).  I'm hoping to achieve a matt dark grey slate colour (or ideally shades thereof).

The polystyrene is then glued to the inside of the tank with silicone aquarium sealant.  The size of the 'wall of rocks' will be 7ft x 2 ft with depths of up 3 inches.

Researching on the web shows others have done this but I'm a novice in terms of resins and am not sure of the products available and sutable for this.  Looking at your products, I'm guessing if anything is suitable in terms of my planned process, it'll be the Epoxy Coating Resin?

Are any of your epoxies and dyes aquarium-safe (usually anything ok with potable water is fine)?

I'm hoping you can recommend resins, dyes and approx. amounts (I appreciate the latter will be a guesstimate! to the nearest pack size will do). Also I get the feeling the resin dries to a gloss finish - any techniques to reduce the gloss effect also appreciated.

Thanks in advance
 
Hiren.
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
To reduce the gloss you can just flat them down using sandpaper.

To calculate how much you need is a bit more difficult, although generally for a good coating we recommend about 1kg of Epoxy Coating Resin for each square meter of surface coverage.

In terms of using in water, you MUST ensure the part is fully cured before putting it into water. Uncured liquid epoxies are almost always toxic in one form or another. The
Epoxy Coating Resin is dangerous for the aquatic environment uncured.  I recommend you leave it at least a couple of weeks to cure, preferably getting some warmth onto it to cook it off.

Also be aware that some pigments and dyes use lead and other heavy metals in them.  My recommendation is to ensure your last coat of resin is a plain undyed coat that way any dyes that could be hazardous to the fish are sealed in.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search