I seem to remember that West Systems stated that their Epoxy is "aquatic -life safe" after a minimum of 1 month at room temperature.
They stated that their epoxy will remain safe up to 60 degrees Celcius, after the recommended 1 month post cure.
Since EC epoxies ar Bisp-A phenolic resins like the West Systems types, they should be the same for practical purposes.
Post curing at slightly elevated temps, maybe using an electric blanket, will of course shorten that period a lot.
Btw .. Warren, I have actually managed to get a sample of West systems Resin cured perfectly using EC fast hardener ... and using the EC recomended mixing ratio, which incidentally is the same as the WS ratio ... (I had run out of normal WS fast hardener
)