Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
How would you set up vac/feed on this shape?
How would you set up vac/feed on this shape?
Post Reply
Like
2
How would you set up vac/feed on this shape?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
jamesw
jamesw
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
I've come to infuse a part with a shape that's not as straightforward as the rectangular parts I've made so far - looking for suggestions on how to set up (It's pretty flat, this is the view from top)
was thinking of feeding from the right side, and pulling vacuum from the upper 2/3's on the left... Or am I better off center feeding the resin?
Reply
Like
2
Reply
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
I would have the resin feed in the middle of the right hand side with the spiral running the full length and the vac outlet in the middle of the left side (so directly opposite) If you have the resin feed in the middle of the part you can get print through on the "seen side" of the part where the resin was fed in.
Just my preference
Carbon
Copies Ltd
Edited
12 Years Ago by
wozza
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How would you set up vac/feed on this shape?
jamesw
-
12 Years Ago
I always infuse from the center and pull vacuum all around the mold.
_GABBER
-
12 Years Ago
I do it the same way as Gabber ;)
matthieutje65
-
12 Years Ago
I would have the resin feed in the middle of the right hand side with the spiral running the full...
wozza
-
12 Years Ago
Wozza, am I going to waste a ton of resin when it reaches the left across the middle where the...
jamesw
-
12 Years Ago
I would infuse from the full left sideto the full right side. Remember the liquid always takes the...
fgayford
-
12 Years Ago
[quote][b]fgayford (16/05/2013)[/b][hr]. I personally do not like to feed from the middle because it...
Nick Igoe
-
12 Years Ago
[quote]...you wrap your feed pipe in flow medium leaving a 6" overhang which you then spraytak or...
stuart321
-
12 Years Ago
I used a spiral feed pipe for my infusions and it is easy to join two or more lengths. It is...
Nick Igoe
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search