need some help after resin infusion


Author
Message
kaperomako
kaperomako
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 199
kind attention.  need some help about "cleaning" out the residues let by the 3m composite spray glue. although my part is not 100% finish, i will like to try the process that matthieutje65 use for his carbon fiber helmet. but i was wondering if this residue will be annoying and get my part ugly.

can anyone help me with what to use in order to clean up my part.
Attachments
IMG-20130422-01738.jpg (223 views, 256.00 KB)
IMG-20130422-01740.jpg (198 views, 406.00 KB)
IMG-20130422-01742.jpg (187 views, 394.00 KB)
IMG-20130422-01741.jpg (179 views, 432.00 KB)
IMG-20130422-WA006.jpg (193 views, 81.00 KB)
IMG-20130422-WA005.jpg (199 views, 112.00 KB)
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi, kaperomako

I had a similar problem.
So I've used a gluespray called "Aerofix 2" to stick the first layer onto the mould.
When I demoulded I had some dry spots and a strange finish.
It still guessing but I think the strange finish is caused by an over-use of sprayglue.
The dryspots are due to the fact their was a small leak in the bag so presure was lost and I had some dry spots.

How I solved it;
Clean the part with some hot-water and a bit of soap.
Use some washing alcohol (NOT ACETONE).
This should remove a big part of the sprayglue.

After that I've sanded the part with different sanding grids.
Add some new coats on top of it
Sand in between the coats and pollish.
You should get a nice finish Wink

Lots of work, but at least you still have your part with a good finish.
How you could solve all of this?! use a gelcoat if weight is not important.
My plan was to go as light as possible so gelcoat would have been an extra weight.

Hope this helps you a bit, Feel free to ask more questions if needed!


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




kaperomako
kaperomako
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 199
thanks for your answer, will try this asap! let's see how it goes around.
kaperomako
kaperomako
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 199
well matthieutj65, you have been  very helpful.  keep posting my advance in the project.

well although the final part did not when 100% like a pro. for my 1st time, i think it when very well. the process takes time but the results and the knowledge acquire was very exciting.  the last part of the engine cover is the holes that attach it to the engine. i am thinking of pasting some insert or any advice??
Attachments
IMG-20130430-01802.jpg (187 views, 398.00 KB)
IMG-20130430-01801.jpg (224 views, 478.00 KB)
IMG-20130430-01798.jpg (187 views, 317.00 KB)
IMG-20130430-01796.jpg (201 views, 423.00 KB)
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you're welcome! looks like a job well done!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search