By kaperomako - 4/22/2013 9:48:12 PM

kind attention.  need some help about "cleaning" out the residues let by the 3m composite spray glue. although my part is not 100% finish, i will like to try the process that matthieutje65 use for his carbon fiber helmet. but i was wondering if this residue will be annoying and get my part ugly.

can anyone help me with what to use in order to clean up my part.
By matthieutje65 - 5/1/2013 8:24:10 PM

you're welcome! looks like a job well done!