Resin Infusion
»
Where can O find the spray that stick the fabric to the mould ?
Where can O find the spray that stick the fabric to the mould ?
Post Reply
Like
3
Prev
1
2
3
4
Next
Jump To Page
Where can O find the spray that stick the fabric to the mould ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
alebassa
alebassa
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 48,
Visits: 171
What a reseller in Italy told me is that stayz was going to cure in the cans in two weeks time. So they had really short shelf life so they stopped selling until they could find a solution for this!
Alessandro
Reply
Like
3
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
thank you Gropius
Reply
Like
3
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
alebassa (04/04/2013)
What a reseller in Italy told me is that stayz was going to cure in the cans in two weeks time. So they had really short shelf life so they stopped selling until they could find a solution for this!
Interesting,
2 weeks is short time indeed. Hope they will fix this. 2 months would be more acceptable.
thank you for the info
Reply
Like
3
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
This is the stuff I've been using
http://www.ecfibreglasssupplies.co.uk/p-2214-aerofix-2-spray-adhesive-500ml.aspx
Only need to use it VERY lightly. Also been using it by rolling out a length of carbon, giving it a very light mist and it holds its shape when cut, not quite as drapable as pro finish but the same level of neat cutting
Reply
Like
2
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
ajb100 (05/04/2013)
This is the stuff I've been using
http://www.ecfibreglasssupplies.co.uk/p-2214-aerofix-2-spray-adhesive-500ml.aspx
Only need to use it VERY lightly. Also been using it by rolling out a length of carbon, giving it a very light mist and it holds its shape when cut, not quite as drapable as pro finish but the same level of neat cutting
Could you tell whether it is epoxy-compatible lke zyvax sprayZ ? Did you experienced any unwanted side-effects ?
thanxx
Reply
Like
2
baja_patient
baja_patient
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
Could we get some info from EasyComposites to regarding the in-can shelf life of StayZ? I have used mine twice and it has since been standing for close to a 8 months. I would be quite dissapointed to find it has gone off, due to the price of it and that it is not available. The results were very good.
Apart from that, I have found a product from 3M with similar specifications. I have not had any experience with it, but maybe EC can give some insights, get some samples and maybe add it to the range?
http://www.merrittsupply.com/products/32055-3m-adjustable-composite-positioning-system-11095-24-oz-spray-can-pn-63291.aspx
cheers
Reply
Like
3
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
Why the hell did I miss that 3M product !?
Sounds perfect !
Where can we find it in Europe ?
Reply
Like
3
Manu
Manu
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 23,
Visits: 435
Hi I have a good story about the spray adhesive, seeking Stayz discovered that the distributor for Europe was less than 70km from my city, I contacted them and they said they had saved hundreds of spray they could not sell because they were defective, that if I wanted to try them gave me one. When I visit his shop to catch the spray. Indeed its spray is defective, to used once, the next day it was all stuck and useless. From then probe different products and brands, it is certainly my choice spraymount 3m, and I have made many infusions and the result is perfect, even among gc50 gelcoat and the first layer of carbon fiber.
www.ktuning.es  
https://www.facebook.com/Ktuning.es/ 
www.carboncycleparts.com 
https://www.facebook.com/CarbonCycleParts/
Attachments
P4060087.jpg
(
391 views,
4.00 KB
)
P4060089.jpg
(
395 views,
18.00 KB
)
Edited
12 Years Ago by
Manu
Reply
Like
3
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
OK.
By the way, I live in Europe (near Paris) and this week I've tried to be delivered a box of 3M ACPS from US retailers, but it is impossible. They are not allowed to ship it this way
Reply
Like
3
prsw
prsw
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 112,
Visits: 1K
I have tried "Infutac" from french Diatex, holds thing in place nicely but leaves fiber trace on the mold surface that has to be wet sanded to remove,
maybe I use alittle to much, or leave in on to long before infusing, dont know, but it has given me a whole lot of extra job.
http://motoform.blogspot.se
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
3
4
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search