wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Another weekend spent shaping foam and sanding body filler!! A good few coats of high build primer. A flat and polish tomorrow and should be able to take a mould from it.
Warren
Carbon
Copies Ltd
Edited
12 Years Ago by
wozza
Reply
Like
2
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Looking good! Your own variation of the NACA duct I guess.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
tauruck
tauruck
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 5
It looks good so far. That part looks like the duct used on NASCAR windows.
Reply
Like
3
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Thanks for the comments chaps. I managed to pull a GRP test piece today just to prove the mould. The duct is for a customer who wanted a specific size Intake Duct. 300mm x 220mm to take 75mm Ducting.
Looks like I will be ordering some Pre Preg don't fancy trying to infuse it.
Warren
Carbon
Copies Ltd
Reply
Like
3
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
wozza (25/03/2013)
Thanks for the comments chaps. I managed to pull a GRP test piece today just to prove the mould. The duct is for a customer who wanted a specific size Intake Duct. 300mm x 220mm to take 75mm Ducting.
Looks like I will be ordering some Pre Preg don't fancy trying to infuse it.
Warren
Quality work Warren.
Reply
Like
3
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Managed to get the plug done for the top section of the Duct which will house the cone filter. The CFD simulation indicates a decent "Ram Air" effect but only a session on the dyno will see if there is any increase in Horse Power.
Carbon
Copies Ltd
Reply
Like
3
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Managed to get the prototype duct finished.
Carbon
Copies Ltd
Reply
Like
2
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
That looks excellent , did you use infusion Warren ?
Chris
Reply
Like
2
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Hi Chris, this one was wet laid but future ones will be done by Infusion. I don't do much wet lay these days
Warren
Carbon
Copies Ltd
Reply
Like
3
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Hi Wozza
Looks nice. How did you do the graphics exactly?
Thanks
Fred
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
1
2
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search