Just used your fishing pole repair kit and got to say it worked great. Instead of polishing I finished my repair with a thin coat of resin but must have under estimated the hardener as after 24 hours it is still tacky. What can I do to resolve this?
Reply
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi

Scrape off the goo and wash off the rest with acetone. Scuff and re-apply properly mixed epoxy.

Epoxy shows no mercy when not mixed in exact proportions like polyester does.

Been there done that.

Hope this helps.

Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search