By Fisherman - 3/31/2013 12:39:37 PM
Just used your fishing pole repair kit and got to say it worked great. Instead of polishing I finished my repair with a thin coat of resin but must have under estimated the hardener as after 24 hours it is still tacky. What can I do to resolve this?
|
By Warren (Staff) - 4/3/2013 3:33:18 PM
Yes that should be fine. Acetone will break down uncured and partially cured resin so it should help you recover the part.
|
|