This is just quick one regarding peel ply finish for secondary bonding,usually a matt finish is left but on the part I pulled today a satin finish was left question is is this good enough for bonding or will sanding be nessisary.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
normally peel ply is made for that, 
For easy removal of infusionmesh or breather & perforated film.
It"s also used to prepare the surface for a next coat of resin/layer of material. 

so it should be ok without sanding...

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search