Peel ply finish
Peel ply finish
Post Reply
Like
3
Peel ply finish
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Shaneer22
Shaneer22
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 156,
Visits: 14K
This is just quick one regarding peel ply finish for secondary bonding,usually a matt finish is left but on the part I pulled today a satin finish was left question is is this good enough for bonding or will sanding be nessisary.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
normally peel ply is made for that,
For easy removal of infusionmesh or breather & perforated film.
It"s also used to prepare the surface for a next coat of resin/layer of material.
so it should be ok without sanding...
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search