This is just quick one regarding peel ply finish for secondary bonding,usually a matt finish is left but on the part I pulled today a satin finish was left question is is this good enough for bonding or will sanding be nessisary.
By matthieutje65
-
3/10/2013 1:09:03 AM
normally peel ply is made for that,
For easy removal of infusionmesh or breather & perforated film.
It"s also used to prepare the surface for a next coat of resin/layer of material.
so it should be ok without sanding...