How to make carbon tube ?


Author
Message
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
I need to make some carbon tube and suspect i need to make a mandrel in the lathe to lay the carbon over, what would be the best material for the mandrel ? i have some nylon and alloy bar, would i have any release issues ?

Thanks in anticipation

Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Reply
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Warren

All layers in one go and wet, the product on the back of the pro finish was making it unwind if that makes sense, it did not help that the tube dia is quite small. I will have another play over the weekend and as the dia is small i am not creating too much scrap.

Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbonfibreworks - 12 Years Ago
matthieutje65 - 12 Years Ago
Drew Diller - 12 Years Ago
carbonfibreworks - 12 Years Ago
prsw - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
tauruck - 12 Years Ago
Drew Diller - 12 Years Ago
BoostSamurai - 12 Years Ago
matthieutje65 - 12 Years Ago
Drew Diller - 12 Years Ago
carbonfibreworks - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search