By carbonfibreworks - 2/26/2013 6:54:19 PM
I need to make some carbon tube and suspect i need to make a mandrel in the lathe to lay the carbon over, what would be the best material for the mandrel ? i have some nylon and alloy bar, would i have any release issues ?
Thanks in anticipation
Chris
|
By carbonfibreworks - 4/25/2013 7:10:19 AM
Thanks for the great tips, i tried using an alloy bar with reasonable results but will try some of the other methods next time.