Group: Forum Members
Posts: 34,
Visits: 837
|
As the subject says....Is it possible to infuse a part with non infusion resin. I have a part I would like to infuse this weekend but the company I ordered more resin from did not ship on time so I wont get the resin until
Monday. The part is fairly small and only takes 3-4 min tops to infuse with infusion resin. I was thinking maybe just add extra infusion mesh. I don't want to wast the material if it just won't work. The resin I am using is not easy composites resin. I wish I could buy all my supplies from easy composites but it not cost effective. IF it matters which it might....I am using the 6mm tubing for my infusions.
Thanks,
Dennis
|