Thanks all for the replies.....I did not try it. I had plenty to do to keep me busy this weekend. (got 28 inches of snow). Plus was able to do some other things on the car that needed to be done. I should have the correct resin today and will make the parts I need this week so I have them for next weekend. The worst part of not being able to make the part I really needed was that I had enough resin but was 20grams short on hardener.
The viscosity of the two resins I have are:
Infusion resin 150cps, Laminating Resin 600cps So not sure how it would have worked but I didn't want to take the chance.