As the subject says....Is it possible to infuse a part with non infusion resin.  I have a part I would like to infuse this weekend but the company I ordered more resin from did not ship on time so I wont get the resin until

Monday. The part is fairly small and only takes 3-4 min tops to infuse with infusion resin. I was thinking maybe just add extra infusion mesh. I don't want to wast the material if it just won't work.   The resin I am using is not easy composites resin. I wish I could buy all my supplies from easy composites but it not cost effective. IF it matters which it might....I am using the 6mm tubing for my infusions.

Thanks,

     Dennis 
By Dennis G - 2/11/2013 4:54:24 PM

Thanks all for the replies.....I did not try it. I had plenty to do to keep me busy this weekend. (got 28 inches of snow). Plus was able to do some other things on the car that needed to be done. I should have the correct resin today and will make the parts I need this week so I have them for next weekend. The worst part of not being able to make the part I really needed was that I had enough resin but was 20grams short on hardener.

The viscosity of the two resins I have are:

Infusion resin  150cps,     Laminating Resin 600cps    So not sure how it would have worked but I didn't want to take the chance.