As the subject says....Is it possible to infuse a part with non infusion resin.  I have a part I would like to infuse this weekend but the company I ordered more resin from did not ship on time so I wont get the resin until

Monday. The part is fairly small and only takes 3-4 min tops to infuse with infusion resin. I was thinking maybe just add extra infusion mesh. I don't want to wast the material if it just won't work.   The resin I am using is not easy composites resin. I wish I could buy all my supplies from easy composites but it not cost effective. IF it matters which it might....I am using the 6mm tubing for my infusions.

Thanks,

     Dennis 
Reply
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
what Warren told me you can not do this as infusion resin like water and simply resin like marmalade it not gonna flow and fill everything.
Edited 12 Years Ago by TomDesign
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search