Hello Matt
I have a question about the EasyPreg surfacing layer. What would happen if I only used one layer of the EasyPreg Surfacing layer and not a backing layer? Would it cure as if it were a one layer of 3k twill infused?

The reason I ask is that I have an absolutely impossible piece to make. If I could apply one layer of the easy preg and cure it I should then be able to treat the surface like I was skinning a part. Because my part is so small skinning will not work, but the easy preg looks like i could cut it into very fine detailed pieces with my surgical scissors and then it would hopefully glue down to my mock up. I would skin my mockup with the easypreg to take its shape and then remove and build up layers for strength on the inside of the part. Then I would use my skinning epoxy to finish the out side surface. Clear/Polish/done!

Thanks

Fred
Replies
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
give us some feedback when finished Fred,
you made me curious about your masterplan!

making something like this forged carbon?
https://www.youtube.com/watch?v=LL7kTnZmExY

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Yes Matt

From one supreme being to another. I will.

How did we become supreme beings anyway. I only have one year of College?

Fred
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Haha, great looking forward to see it fred.
That is indeed very strange cause I'm STILL in college :p
guess it's spending a lot of time on here, more interesting than spending time on facebook or twitter BigGrin

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com