Hi All,

I guess I work my little dremel hard but it just died the other day Sad
I have often wondered if the dust from working composites is bad for them and if it the cause of death in this case ?

(I wonder if I should get a new model with flexible drive to keep the motor more out of the dust ?)

Am I right, any comments, suggestions etc ?

Cheers,
Richard B.
Tags
Daz
Daz
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 93, Visits: 651
RBailey (22/01/2013)
Hi All,

I guess I work my little dremel hard but it just died the other day Sad
I have often wondered if the dust from working composites is bad for them and if it the cause of death in this case ?

(I wonder if I should get a new model with flexible drive to keep the motor more out of the dust ?)

Am I right, any comments, suggestions etc ?

Cheers,
Richard B.
I also killed mine .

took it apart and it was full of the dust

Dont know jf this was the cause as it was very new..
baja_patient
baja_patient
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Daz, as you said, it was new and full of dust and that killed it.

Carbon dust is highly conductive, you don't want that in and around your electronics. Most likely it shorted it out. You could clean it all up and try if it works, but unlikely.

Getting the flexible shaft is a good idea, got that and the dremmel is further away from the workpiece. Also I always work with some form of extraction to suck up the dust as it is created.

gd luck
NikCFC
NikCFC
Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)
Group: Forum Members
Posts: 61, Visits: 871
Always use the flexible shaft when cutting carbon and polyester parts and keep the main unit higher - away from the dust. Had to destroy a dremel to learn.
Daz
Daz
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 93, Visits: 651
I have a flexi shaft now for the new one.
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As Already said, Carbon dust is a killer. Our Dremel is kept high up with a long flexible shaft to keep the cutting away from the motor and it has lasted fine.

Carbon dust can damage many electrical goods.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
_GABBER
_GABBER
Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)Supreme Being (465 reputation)
Group: Forum Members
Posts: 41, Visits: 646
I use a dremel and a saw fein. I always use vacuum cleaner near the blade
fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Probably a good idea to blow out your dremel with compressed air every once in a while.

Fred
NikCFC
NikCFC
Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)
Group: Forum Members
Posts: 61, Visits: 871
I'd also suggest to blow out the dust but keeping in mind that you have to remove the dust away from the dremel by keeping the line a bit further and away from the vents. If you blow the dust without care you might push the dust further inside the motor which will make thing worse.
pk_090
pk_090
Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)
Group: Forum Members
Posts: 47, Visits: 169
A compressor and air tools are not really expensive compared to conventional mains dremel and alot safer! Just just require slight oiling thought the air inlet pipe daily and the should last a long time! So much safer as they wont short out too. I always has a vacuum cleaner as close to the blade as i can sucking in the dust, but i cant seem to find a vaccum cleaner that is none electrical so i have just sealed all the gaps up with silicone.  