Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
Elastifilm and pre-preg
Elastifilm and pre-preg
Post Reply
Like
3
Elastifilm and pre-preg
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Extreme
Extreme
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 17,
Visits: 78
Hi there,
Just wondering if Elastifilm can be used with pre-preg layups?
thank you, Erick
Reply
Like
3
Kevin-Lee
Kevin-Lee
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 44,
Visits: 2.4K
Hi,
From what I understand Elastifilm is only intended for prepreg layups and/or as a replaceable membrane on a vac table. So I would say that the answer to your question is yes, it can be used for prepreg...
Kev.
Reply
Like
2
baja_patient
baja_patient
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
From what I have read it is not ideal for resin infusion, due to its highly elastic nature it fills the cells of the flow media, thus inhibiting resin flow.
Reply
Like
3
crud249
crud249
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 9
I have used elastifilm in resin infusion and it works very well, the problem with it is it sticks to the laminate after so you have to use a peel ply or release film. Where as normal vac bag peels off.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search