I suspect that cap is made in 3 parts, the back retaining plate, a pressed plate containing the design, and then a clear dome of plastic or resin on top. If the clear bit is soft enough to dig into, then chances are they just used a traditional "doming" process with a PU doming resin to create that part. But if rigid, it could be an injection moulded part,
I would probably do it in a similar process. If you want to cast the clear section, then a 2 part mould to include the domed front face and the logo impression on the back would work. You could even paint the reverse to do the colours meaning you can knock it down to a 2 part piece as you then just need the retaining plate.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|