Group: Administrators
Posts: 167,
Visits: 4.6K
|
Hi RedRocket; the Breather Fabric is something which we constantly consider as to whether it should or shouldn't be included within the kit. For some projects, as per MarkMK's suggestion, it is used along with or instead of a resin break to act as a soaker or alternatively, and the predominant reason why it is in the kit, when envelope bagging or if you have any sharps (botls, nuts, fasteners, etc.) then the breather cloth can be used to protect agaisnst puncturing the vacuum bag - You're right to question though as for most Resin Infusion processes, it won't be necessary.
|