andygtt - 8/18/2020 3:11:19 PM
I made a new design of dash recently for my car (noble M12)... started as little more that filler and cardboard so shows what can be done with a cheap and dirty buck (if your quick and careful).
Ive included pictures of the final product (some of them before they had been flatted and final lacquered), but also some buck pictures so people can see how the shapes were created, maybe give some motivation for those that think it takes more skills than it actually does.




















here is an original noble dash for comparison


Looking really nice. Which method did you use for the carbon part i.e wet layup, infusion etc?

Classicarbon
C
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 86, Visits: 639
VW engine lid. Infiusion.

Coldever
C
Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)Supreme Being (174 reputation)
Group: Forum Members
Posts: 12, Visits: 187
I finished my carbon recumbent bike this summer. Made a set of molds from cnc-machined plugs. Frame was wet laminated under vacuum in two halves then joined. Stem and various other smaller carbon parts were made with the help of 3d-printed molds and cores.

P8200026-2pieni by Mikko Hörkkö, on Flickr

PA270178-2 by Mikko Hörkkö, on Flickr

Edited 6 Years Ago by Coldever
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Nice job, a lot of work in that and it turned out really nice.

Thats a hell of a chain!
Richard webb
R
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 1, Visits: 25
Classicarbon - 9/21/2020 2:07:59 PM
VW engine lid. Infiusion.

Nice, I have made a VW engine lid to Smile  

Edited 6 Years Ago by Richard webb
Ken Olson
Ken Olson
Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)
Group: Forum Members
Posts: 8, Visits: 41
Here is a model boat I did with some red kevlar/carbon fabric. Turned out pretty good. Resin infused with 5.7 oz carbon, 2mm soric core and then this honeycomb on the outside.  







Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Looks pretty good and the honeycomb pattern fabric is pretty rare these days. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Legoman
Legoman
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 29, Visits: 622
GSX-R 600 lower fairing. Vacuum Infusion.



Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Those parts are looking good. Much lighter than the originals?

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant