Hy guys. 
I work on a project that requires wraping wooden tapered ellipsoid object in 2 layers of carbon fiber. Carbon is added for stiffness and visual appearence so nice layup is must.

Carbon goes from bottom of part and goes on sides, it doesnt go all the way around.

I have to use wet layup method combined with vacuum so my plan is to:
1. Cover wood with black tinted epoxy
2. Wait for tacky stage and add first layer
3. Add resin to saturate fabric
4. Wait for tacky stage to add other layer
5. Add resin to saturate fabric
6. Place peel ply and breather and use around 20% vacuum to remove excess resin

My questions are:
1. Will 20% vacuum remove excess resin since most of resin reached tacky or beyond tacky stage?
2. Is there anything to change in the process to ensure good bond and appearance?
3. Process is like skinning with carbon only using 2 layers instead of one and using vacuum to remove excess resin. Should I do like plan above or should I do 1 layer, wait it to cure, key whole surface and repeat process for 2nd layer?

Thanks Smile
Reply
Dentex
D
Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)
Group: Forum Members
Posts: 42, Visits: 1.4K
https://ibb.co/g6ht9Mk
https://ibb.co/Rz0MSx6
https://ibb.co/g7Mh6D1
https://ibb.co/QYbt5wq
https://ibb.co/rv45znP
https://ibb.co/ZHm8BJp

There you go guys. Object is actually speargun body and bottom part is that where 2 holes can be seen. Not entire body needs to be wraped, only bottom and sides where most hits and scratches will occur from rocks.

Any extra resin is problem because it will affect buoyancy and thats the main reason why I consider vacuuming it. Also there are some slight curves that might be better done using vacuum.

If this was one layer skinning I think it could be done as regular wet layup skinning, but it needs to be visually nice and with as less as possible extra weight with 2 layers. I am afraid that if I go with layup without vacuum, fabric might float on resin and it will create mess that will be very hard to sand without destroying wooden part.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dentex - 4 Years Ago
Fasta - 4 Years Ago
Dentex - 4 Years Ago
explorecomposites - 4 Years Ago
Warren (Staff) - 4 Years Ago
Dentex - 4 Years Ago
Dentex - 4 Years Ago
oekmont - 4 Years Ago
Hanaldo - 4 Years Ago
Dentex - 4 Years Ago
Fasta - 4 Years Ago
Dentex - 4 Years Ago
Fasta - 4 Years Ago
Hanaldo - 4 Years Ago
Dentex - 4 Years Ago
Fasta - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search