+x torsten Ker - 11/5/2020 10:26:21 PMyes, you are right, that may work but I think not to make the mould to stiff and be carefull not to crack the gelcoat on demoulding
+x torsten Ker - 11/5/2020 10:10:47 PMI guess the bag hat to be rigid and think you will have no other choice to make 5 part mould, each side and bottom or it will be a challenge to get the saddlebag outThe problem is the straight sided and the overlap on the bottom to one side