have you thought about doing 2 parts , angeling the sides/rounding and glueing them together with glassfibre tape One mould for the back and one for the font A single multipart usuable mould will be a lot of work
You could then sand off the seam edges, fill them abit and spray the lot much easier that way
I did that on 1989 for bike saddle bags with polyester and hand layup :-)
|