Group: Forum Members
Posts: 468,
Visits: 2.7K
|
I reuse bags all the time (pikey I know). I do tend to hand lay and vac. I seal up one end of the bag with gum tape, put my mould/part in and seal up the open end with gum tape. I leave the breech unit in the same place and just put in a strip of breather to pull air out. Once done I pull the bag open at the tape, remove the old tape then just use new tape next time. Obviously this is only one end. I dont think this woould work well with infusion due to the careful placement of the resin / vac pipes.
I probably get 10 uses out of a bag before its looking battered. It still holds vacuum but I tend to replace it if its looking this way.
|