Talk Composites - The Forum for Advanced Composites

vacuum bag that can be used more than once

http://www.talkcomposites.com/Topic3901.aspx

By mhdghoul - 12/19/2012 1:42:28 PM

guys , have any of u made a vacume bag that can be used multiple times , if yes , or u have an idea about it , please say , and show some picks too if u have , i really appreciate that,

thanks anyway everybody.

mhd ghoul
By brasco - 12/30/2012 9:35:58 PM

Smooth On has some very awesome tutorials. that gun to spray rubber is about 800 USD and the cartridges come i think 4 per box. it is very efficient on rubber and mess in general,and the "bag" can be re used many many times. the bag thickness is 1/8 to 1/4 inch ( 3 to 6 mm roughly)
and are then paired up with its custom made mold. initial cost is high,but the material savings and waste generation will be good on your budget.
Smooth On bonnet skin tutorial is a good one to illustrate making the re useable bag.