Smooth On has some very awesome tutorials. that gun to spray rubber is about 800 USD and the cartridges come i think 4 per box. it is very efficient on rubber and mess in general,and the "bag" can be re used many many times. the bag thickness is 1/8 to 1/4 inch ( 3 to 6 mm roughly)
and are then paired up with its custom made mold. initial cost is high,but the material savings and waste generation will be good on your budget.
Smooth On bonnet skin tutorial is a good one to illustrate making the re useable bag.


CarbonFiberCreations



fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
I have read and seen somewhere on the web a reusable bag made out of latex rubber. If I remember right they were from the USA and were called Boa Bags. They conformed very nicely to most shapes. I think they can only be used for wet bagging and not infusion. They also could make custom bags out of latex over a mandrel shape you provided so you could do closed molded pressurized parts (bladder molding) .This could be infused.

Worth looking into. I will revisit this technic some time in the future because I want to make parts similar to what the cycle industry does. Some us a bladder to push the internal carbon to the out side surface of the mold.

Fred     
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I should add that I make bags rather than the pleated tents that are favoured for infusion.  Does this make sense?
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I reuse bags all the time (pikey I know).  I do tend to hand lay and vac.  I seal up one end of the bag with gum tape, put my mould/part in and seal up the open end with gum tape.  I leave the breech unit in the same place and just put in a strip of breather to pull air out.  Once done I pull the bag open at the tape, remove the old tape then just use new tape next time.  Obviously this is only one end.  I dont think this woould work well with infusion due to the careful placement of the resin / vac pipes. 

I probably get 10 uses out of a bag before its looking battered.  It still holds vacuum but I tend to replace it if its looking this way.
mhdghoul
mhdghoul
Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)
Group: Forum Members
Posts: 49, Visits: 113
THANK U , I ALREADY KNOW ABOUT THAT , BUT THIS IS FOR A SPECIFIC MOLD I NEED A UNIVERSAL ONE , I ALREADY MADE A BIG BAG AND EVERY TIME I CUT ONE SIDE AND RECLOSE IT , BUT CANNOT USE IT MORE THAN 3 TIMES Smile

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
This is how you should do it...

 

is next on my to do list Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




mhdghoul
mhdghoul
Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)
Group: Forum Members
Posts: 49, Visits: 113
guys , have any of u made a vacume bag that can be used multiple times , if yes , or u have an idea about it , please say , and show some picks too if u have , i really appreciate that,

thanks anyway everybody.

mhd ghoul

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Edited 13 Years Ago by mhdghoul
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search